Low carbon steel shot is produced using selected low carbon, sulphur and phosphorus content scrap.
After the melting process, steel shot are produced by melting in the induction furnaces, at about 1600-1650 °C, which are automized, followed by quenching process, are crack free with a bainitic microstructure.
High carbon steel shot is produced from scrap all kinds of hard, brittle martensite microstructure have surface cracks and causes heat treatment applied after casting.
The service life of Tosçelik Granul low carbon steel shot has 20% longer life than high carbon steel shot. Tosçelik Granul low carbon steel shot, with its long life and high hardness, shows excellent performance in removal of sand, scale and rust, deburring, surface preparation and shot peening process.
It is ideal for the use in foundries, forges, ironworks, rolling mills, machine building shops, in steel industry, in automobile and aircraft industries as well as in structural steel industry.